Technical Parameter
GB/T 17643-2011
No. |
Item |
Index |
||||||
Thickness mm |
0.75 |
1.00 |
1.25 |
1.50 |
2.00 |
2.50 |
3.00 |
|
1 |
Density g/cm³ |
≥0.940 |
||||||
2 |
Tensile yield strength (longitudinal and transverse) N/mm |
≥11 |
≥15 |
≥18 |
≥22 |
≥29 |
≥37 |
≥44 |
3 |
Tensile fracture strength (longitudinal and transverse) N/mm |
≥20 |
≥27 |
≥33 |
≥40 |
≥53 |
≥67 |
≥80 |
4 |
Tensile yield strain (longitudinal and transverse) % |
≥12 |
||||||
5 |
Tensile fracture strain (longitudinal and transverse) % |
≥700 |
||||||
6 |
Right angle tear load (longitudinal and transverse) N |
≥93 |
≥125 |
≥160 |
≥190 |
≥250 |
≥315 |
≥375 |
7 |
Puncture resistance strength N |
≥240 |
≥320 |
≥400 |
≥480 |
≥640 |
≥800 |
≥960 |
8 |
Tensile load stress cracking h |
≥500 |
||||||
9 |
Carbon black content % |
2.0~2.8 |
||||||
10 |
Carbon black dispersibility |
Among 10 data, there should be no more than 1 level 3, and levels 4 and 5 are not allowed. |
||||||
11 |
Oxidation induction time(OIT) min |
Induction time of atmospheric pressure oxidation ≥100 |
||||||
Induction time of high-pressure oxidation ≥400 |
||||||||
12 |
85 ℃ thermal aging (retention rate of atmospheric pressure OIT after 90 days) % |
≥55 |
||||||
13 |
UV resistance (OIT retention rate after 1600 hours of UV irradiation) % |
≥50 |